Material
14Cr17Ni2 ESR forging
Heat treatment
Quenched & tempered HRC 23–28
Ground bore & OD
Φ80 (+0.030/+0.013) · Φ155.5 (+0.02/0)
Runout & teeth
≤ 0.01 mm runout · 60 toothed locations across the end faces

Component role and replaceable-insert design

This cutter body is used in single-shaft and twin-shaft solid-waste shredders with replaceable carbide cutting inserts. The process sheet records deburring at 60 toothed locations across both end faces.

Machined 14Cr17Ni2 stainless steel shredder cutter body with 60 toothed locations across the end faces and precision ground bore

ESR forging stock and co-treated test coupons

Production starts from electroslag-remelted (ESR) 14Cr17Ni2 stainless steel bar stock (Φ180 mm), sawn into Φ180 × 80 mm single-part blanks. Dedicated chemical-analysis coupons (Φ180 × 10 mm) and mechanical-property coupons (Φ180 × 23 mm) are cut from the same bar—one set tested as-forged and the second co-processed with the cutter batch through HRC 23–28 quenching and tempering.

Multi-stage grinding, mandrel alignment and CNC pocket milling

The process route includes turning, grinding, stress-relief aging and mandrel runout checks. The 60 toothed locations on the end faces are deburred to the process requirements.

Scroll horizontally to compare measurements.
OperationKey dimensional & process controls
00–10 Forging blank & Q&TΦ180 × 80 mm 14Cr17Ni2 ESR blank; rough turn; quench & temper to HRC 23–28 with batch witness coupons
15–30 Turning, surface & ID grindingSemi-finish/finish turn; double-side surface grind to 68 mm thickness; internal grind bore to Φ80 (+0.030/+0.013) mm
40–50 Mandrel cylindrical grindingVerify precision mandrel runout ≤ 0.01 mm; assemble cleaned part on mandrel and grind OD to Φ155.5 (+0.02/0) mm
60–75 Rough CNC, aging & center lappingCNC rough mill tooth profile; thermal stress-relief aging; re-lap mandrel centers to hold cutter OD runout ≤ 0.01 mm
80–90 Finish CNC seat milling & deburringMeasure actual carbide insert lot thickness before finish-milling pockets; dismount and deburr all 60 tooth faces
18-stage machining, heat-treatment and grinding route

Planning a heavy-duty cutter or rotor component

When requesting a quote for multi-tooth cutter bodies or indexed tooling discs, share the forging grade, target hardness range, bore/OD grinding tolerances, runout datum and mating carbide insert tolerances so thermal stress relief and mandrel grinding can be built into the route.

Apply this to your own project.

Share the drawing, quantity and specification you want to review.